Drop a weight onto a flat piece of plastic and see whether it cracks. That is the idea behind Gardner impact testing, and ASTM D5420 turns it into a repeatable measurement of how much energy a rigid plastic specimen absorbs before it fails.
What ASTM D5420 Measures
In the test, a specimen rests over a support, a striker sits on the specimen, and a known weight falls through a guide tube onto the striker. By changing the drop height or the weight, the test finds the energy at which the specimen fails. Because impact failure is statistical rather than a single fixed point, the method uses a staircase approach: each specimen is tested at a height set by whether the previous specimen passed or failed, and the mean failure energy is calculated from the series.
The configuration of the striker and support is described by a geometry designation. The common Gardner configuration gives the test its everyday name, Gardner impact. Thickness, conditioning, and test temperature all affect the energy, so every specimen in a series is prepared and held the same way.
The Staircase Method
A brittle material does not fail at exactly one energy every time. Small differences in the specimen and the strike spread the failures across a range. The staircase method is built for that reality: it concentrates the tests near the energy where about half the specimens fail, and reports the mean failure energy with its variability. A single drop on a single specimen would say very little about the material.
This matters when a specification lists a minimum impact energy. The comparison the reviewer wants is between the specification value and the mean failure energy from a proper series on representative specimens, at the stated thickness and temperature.
Thickness and Temperature
Impact energy depends strongly on specimen thickness, so values are compared at the same thickness. Temperature matters as well. Many plastics that absorb an impact at room temperature turn brittle in the cold, so a part that lives outdoors or in an unheated space often needs impact data at a low temperature as well as at room temperature.
If the production part is thicker or thinner than a standard plaque, or will see winter temperatures, mention it on the request so the specimens and conditioning can be set up to match.
Where Gardner Impact Fits Among Impact Methods
Falling weight impact answers a different question than pendulum impact. A falling weight drives a striker into a flat specimen and reports the energy to failure, which suits sheet, panel, and molded flat parts. Pendulum methods such as Izod and Charpy strike a notched bar and report energy per unit of width or area, which suits notched-sensitivity and material-comparison work. A program that needs both a flat-part impact value and a notched material value runs both.
GPTesting runs ASTM D5420 under A2LA Certificate No. 0079.01, alongside other falling weight and multiaxial impact methods. If your drawing cites a falling weight impact value, confirm the method and geometry on the scope, browse related methods on our tests page, and use our Testing Readiness Checklist to gather the specimens and conditioning details before shipping. If you are unsure which impact method applies, a consultation is a quick way to settle it.
Ready to test? Request a quote, and we will confirm the method and geometry before any specimens are dropped.
Frequently Asked Questions
What is ASTM D5420?
ASTM D5420 is the standard test method for impact resistance of a flat, rigid plastic specimen struck by a falling weight that drives a striker (Gardner impact). It reports the energy at which the specimen fails.
What is the Gardner impact test?
The Gardner impact test is the common name for the falling weight impact configuration used in ASTM D5420. A weight falls through a guide tube onto a striker resting on the specimen, and the test finds the failure energy.
What is mean failure energy?
Impact failure is statistical, so the method tests a series of specimens using a staircase of drop heights and reports the mean failure energy of the series rather than a single reading.
Does specimen thickness affect the result?
Yes. Impact energy depends strongly on thickness, so a value measured at one thickness does not carry over to another. Report the thickness with the result and compare only specimens of the same thickness.
Is ASTM D5420 on the GPTesting scope of accreditation?
Yes. ASTM D5420 is listed under Impact (Falling Weight) on the GPTesting A2LA scope, Certificate No. 0079.01, ISO/IEC 17025:2017.
About GPTesting. Ghesquiere Plastic Testing is a family-owned, A2LA-accredited (Cert #0079.01) materials testing lab in Harper Woods, Michigan, testing automotive materials since 1971.